ISO 19403-1:2022 to ISO 19403-7:2024

Paints and varnishes – Wettability

This standard series specifies optical test methods:

 

  • for the measurement of the contact angle
  • for the determination of the free surface energy of a solid surface, including the polar and disperse parts
  • for the determination of the surface tension of liquids, including the polar and disperse parts
  • for the checking of the measurement arrangement with reference materials

 

It can be applied for the characterization of substrates, coatings, and coating materials. The applicability can be restricted for liquids with non-Newtonian rheology. 

 